A PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC preparation process for cathode material of sodium ion battery comprises the following steps: First, the production line of cathode materials for sodium ion batteries is assembled, and then the sodium salt is mixed with manganese oxide, titanium oxide and nickel oxide in a mixing tank. After mixing, the sodium salt is added to the ball mill and anhydrous ethanol is added for 3-5h ball grinding.


PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC

After ball milling, sieve and dry; The dry mixture is calcined at high temperature under the protection of inert gas for 8-12h, and then cooled to room temperature to obtain the active material; Therefore, PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC field in view of the existing sodium ion battery cathode materials and related preparation devices in the preparation process of the above problems,


what is magnetic separation method for concentration of ore?

This paper presents a PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC preparation process and device which can effectively solve the above technical problems. The purpose is to design a kind of preparation technology and device which can effectively solve the above problems in the preparation process of the anode material of sodium ion battery and the related preparation device.

Contact: DELLA

Mob: +86-13929907491

sales@powtechina.com

Join Us
Contact Us

FOSHAN POWTECH TECHNOLOGY COMPANY LIMITED.

No.9, Factory 2, Shijin Industry Park, Shishan Town, Nanhai District, Foshan City, Guangdong, China
Ph: +86-13929907491
E-mail: sales@ptmsmagnet.com
Website: https://www.ptmsmagnet.com

Copyright © Foshan Powtech Technology Company Limited. All Rights Reserved.   Sitemap   XML