After PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC screening, lithium nickel-cobalt manganate requires the step of iron removal before and after batch mixing to carry out batch mixing homogenization. In the process of feeding, it is necessary to measure the weight in advance, because the change of weight often has a fatal effect on the formula, usually we need to control the error of no more than two thousand.
In the equipment for PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC, it is necessary to use alumina ceramics inside the equipment, which has the advantage of preventing REDOX. In the process of loading tons of bags, it is easy to miss the phenomenon in the process, at this time we can choose the lifting manipulator to operate.
Finally, PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC field is required to pay attention to the environment to strictly ensure that there is no dust, the main reason is that in the automatic loading and unloading process, the leakage of dust will lead to the effect of nickel cobalt lithium manganese acid can not meet the predetermined requirements. In addition, it is necessary to ensure the accuracy of weighing. These are the more important matters in the process.
Contact: DELLA
Mob: +86-13929907491