The lepidolite concentrate is manually sent from the concentrate warehouse to the scale plate conveyor by forklift or grab bucket, and then transported to the two-axis mixing and the sulfate used in its matching phase by the metering belt for mixing, and the proportioned mixture is stirred by the agitator and then entered the rotary kiln for calcining. In the calcination section of about 800℃~900℃ temperature of crystalline conversion roasting, in order to PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC removal process.
After cooling in the cooling section, the baking material is discharged from the kiln head, so that the Li2O and SO42- in it are combined into Li2SO4 soluble in water, and acidified clinker is obtained. Then it is cooled to about 60℃ by the cooling machine, and then it is broken by the jaw crusher and sent to the cache in the storage bin. The metering device under the storage bin and the new water before the mill are mixed in proportion and then enter the mill for water quenching and grinding, grinding to about 100 mesh, and the slurry naturally flows into the mixing tank for PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC magnetic removal.
PTMS is the main PTMS magnetic separation equipment professional company, PTMS magnetic separation equipment for kaolin, potassium sodium feldspar, quartz sand removal of iron (Fe2O3). PTMS to provide customers with high quality PTMS magnetic separator, in addition to iron equipment and other products and services, the best choice of PTMS magnetic separator. PTMS develops, designs, and sells mining machinery, iron removal equipment, and dry magnetic separators.
Contact: DELLA
Mob: +86-13929907491