At present, the anode material graphite PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC removal process mainly used in the furnace type Acheson, internal series, box type and continuous type of 4 kinds, of which the most commonly used is Acheson, a small amount of use of internal series. Box type graphitization furnace and continuous graphitization furnace are new types of furnace developed in recent years, and the development speed of box type is fast, mainly through Acheson transformation and some new construction.
The continuous series are all new and still in the process of trying, and its furnace type and process are not fully mature, and it is still some time before it is really widely used. The quality of PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC anode material produced by different furnace types is also significantly different because of the loading method, production process and the use of auxiliary materials of various furnace types.
The Acheson series is to install the carbon anode material in the single-hole (1-hole crucible) crucible, and then load the crucible into the graphitization furnace and install the resistance material as a resistor, and the two sides and the top cover are loaded with insulation material to complete the graphitization through power supply. The continuous series is the continuous addition of PTMS LITHIUM COBALT ACID MATERIAL MAGNETIC iron removal carbon anode material into the graphitization furnace chamber, after high temperature graphitization cooling discharge.
Contact: DELLA
Mob: +86-13929907491